Shopping Cart

No products in the cart.

ASTM-D4273 2005

$40.63

D4273-05 Standard Test Methods for Polyurethane Raw Materials Determination of Primary Hydroxyl Content of Polyether Polyols

Published By Publication Date Number of Pages
ASTM 2005 8
Guaranteed Safe Checkout
Categories: ,

If you have any questions, feel free to reach out to our online customer service team by clicking on the bottom right corner. We’re here to assist you 24/7.
Email:[email protected]

1.1 Carbon-13 Nuclear Magnetic Resonance Spectroscopy(carbon-13 NMR), measures the primary hydroxyl content of ethylene oxide-propylene oxide polyethers used in preparing flexible foams. It is best suited for polyethers with primary hydroxyl contents of 10 to 90 %.

Note 1There is no equivalent ISO standard.

1.2 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

PDF Catalog

PDF Pages PDF Title
1 Scope
Referenced Documents
Terminology
Summary of Test Method
Significance and Use
Equipment
Reagents
Standards
2 Preparation of Sample
Instrument Preparation
NMR Analysis
Calculation
Report
FIG. 1
3 FIG. 2
FIG. 3
FIG. 4
4 Precision and Bias
Keywords
X1. FLUORINE-19 NUCLEAR MAGNETIC RESONANCE SPECTROSCOPY METHOD FOR DETERMINATION OF PRIMARY HYDROXYL CONTENT OF POLYETHER POLYOLS
X1.1 Scope
X1.2 Summary of Test Method
TABLE 1
TABLE 2
5 X1.3 Equipment
X1.4 Reagents and Materials
X1.5 Standards
X1.6 Preparation of Sample
X1.7 Instrument Preparation
X1.8 NMR Analysis
6 X1.9 Mixtures of Polyethers and Chain Extenders
X1.10 Calculation
FIG. X1.1
FIG. X1.2
7 X1.11 Report
X1.12 Precision and Bias
FIG. X1.3
ASTM-D4273 2005
$40.63