Shopping Cart

No products in the cart.

ASTM-D2413:2016 Edition

$35.75

D2413-16 Standard Practice for Preparation of Insulating Paper and Board Impregnated with a Liquid Dielectric

Published By Publication Date Number of Pages
ASTM 2016 4
Guaranteed Safe Checkout
Categories: ,

If you have any questions, feel free to reach out to our online customer service team by clicking on the bottom right corner. We’re here to assist you 24/7.
Email:[email protected]

ASTM D2413-16

Historical Standard: Standard Practice for Preparation of Insulating Paper and Board Impregnated with a Liquid Dielectric

ASTM D2413

Scope

1.1 This practice covers the preparation of insulating paper and board impregnated with a liquid dielectric. Where this practice states only “paper,” the same procedure shall apply to board.

1.2 This practice has been found practicable for papers having nominal thickness of 0.05 mm (2 mil) and above. It has been used successfully for insulating board as thick as 6 mm (1/4 in.) when care is taken to ensure the specimen geometry necessary for valid measurement of dielectric properties. Suitable geometry depends on the electrode system used. Rigid solid opposing electrodes require flat specimens that have essentially parallel surfaces.

1.3 The values stated in SI units are to be regarded as standard. No other units of measurement are included in this standard.

Keywords

board; dielectric strength; dissipation factor; drying; impulse strength; il impregnation; paper permittivity; pressboard; vacuum drying ;

ICS Code

ICS Number Code 29.035.10 (Paper and board insulating materials)

DOI: 10.1520/D2413-16

ASTM-D2413